Sulphur Recirculation CUTNOX NextBAT Sulphur Recirculation for reducing corrosion and increasing electrical efficiency in WtE boilers Dr. Sven Andersson Götaverken Miljö AB, Sweden – a Babcock & Wilcox Vølund company GÖTAVERKEN MILJÖ AB –a Babcock & Wilcox Vølundcompany SSuullpphhuurr RReecciirrccuullaattiioonn CUTNOX NextBAT Operating principles Full-scale operation Ashes and deposits Emissions Corrosion rates Sulphur Recirculation Sulphur in fuel Ash GÖTAVERKEN MILJÖ AB –a Babcock & Wilcox Vølundcompany Sulphur Recirculation CCUUTTNNOOXX NextBAT Operating principles Full-scale installation NO reduction x GÖTAVERKEN MILJÖ AB –a Babcock & Wilcox Vølundcompany Sulphur Recirculation CUTNOX NNeexxttBBAATT HCl / SO / NH 2 3 Hg Dioxins NO x Fine particles Energy recovery Sulphur Recirculation CUTNOX™ in combination with SNCR GÖTAVERKEN MILJÖ AB –a Babcock & Wilcox Vølundcompany SSuullpphhuurr RReecciirrccuullaattiioonn CUTNOX NextBAT Electricity production in WtE is limited by superheater corrosion Biomass or waste fired boiler GÖTAVERKEN MILJÖ AB –a Babcock & Wilcox Vølundcompany SSuullpphhuurr RReecciirrccuullaattiioonn CUTNOX NextBAT Sulphur mass balance Flue gas Sulphur in fuel Ash GÖTAVERKEN MILJÖ AB –a Babcock & Wilcox Vølundcompany SSuullpphhuurr RReecciirrccuullaattiioonn CUTNOX NextBAT Sulphur dosage inhibits corrosion Higher SO concentration: 2 Alkali chlorides → alkali sulphates (corrosive) (non corrosive) Sulphur dosage Flue gas Sulphur in fuel Ash GÖTAVERKEN MILJÖ AB –a Babcock & Wilcox Vølundcompany SSuullpphhuurr RReecciirrccuullaattiioonn CUTNOX NextBAT Sulphur Recirculation for High Efficiency, Low Corrosion WtE Higher SO concentration: 2 Alkali chlorides → alkali sulphates (corrosive) (non corrosive) Sulphur Recirculation Sulphur in fuel Ash GÖTAVERKEN MILJÖ AB –a Babcock & Wilcox Vølundcompany Sulphur Recirculation CUTNOX NextBAT The effect of chromium depletion on chromia forming steels Before After 304L (Fe20Cr10Ni), 5% O + 40%H O, 600°C 2 2 1.4 1.4 Chromate l C formed 1.2 1.2 K )) 22 mm 1.0 cc 1.0 g/g/ mm (( 00..88 n n aiai O3 s gs g 00..66 C ss aa 2 MM 00..44 K 00..22 O (no salt) 2 00..00 4 00 2244 4488 7722 9966 112200 114444 116688 O S EExxppoossuurree ttiimmee ((hh)) 2 K O + H O + KCl 2 2 (Cr,Fe) O Fe O + K CrO + HCl 2 3 2 3 2 4 Pettersson, J., Folkeson, N., Johansson, L.-G., Svensson, J.-E., The Effects of KCl, K SO , and K CO on the High Temperature 2 4 2 3 GÖTAVERKEN MILJÖ AB –a Babcock & Wilcox Vølundcompany Corrosion of a 304-Type Austenitic Stainless Steel. Oxidation of Metals, 2011. 76(1): p. 93-109. Sulphur Recirculation CUTNOX NextBAT The effect of chromium depletion on chromia forming steels Before After 304L (Fe20Cr10Ni), 5% O + 40%H O, 600°C 2 2 1.4 11..44 Chromate l C formed 1.2 11..22 K ))) 222 mmm 1.0 ccc 11..00 g/g/g/ mmm ((( 000...888 n n n aiaiai O3 Chromate s gs gs g 000...666 C formed sss aaa 2 MMM 000...444 K 000...222 O (no salt) 2 000...000 4 000 222444 444888 777222 999666 111222000 111444444 111666888 O S EEExxxpppooosssuuurrreee tttiiimmmeee (((hhh))) 2 K O + H O + K CO 2 2 2 3 (Cr,Fe) O Fe O + K CrO + CO 2 3 2 3 2 4 2 Pettersson, J., Folkeson, N., Johansson, L.-G., Svensson, J.-E., The Effects of KCl, K SO , and K CO on the High Temperature 2 4 2 3 GÖTAVERKEN MILJÖ AB –a Babcock & Wilcox Vølundcompany Corrosion of a 304-Type Austenitic Stainless Steel. Oxidation of Metals, 2011. 76(1): p. 93-109.

Description:
High temp corrosion probe 24 h and 1000 h. Impactor and deposits probe. AMESA continuous dioxin sampler. Emission meas. Sulphur Recirculation
See more

The list of books you might like

Most books are stored in the elastic cloud where traffic is expensive. For this reason, we have a limit on daily download.